NORYL GTX™ Resin 951W (Asia)

Technical Datasheet | Supplied by SABIC
NORYL GTX™ Resin 951W (Asia) is a non-reinforced, heat stabilized, impact modified alloy of polyphenylene ether (PPE) and polyamide (nylon) by SABIC. It offers high heat resistance, melt flow, low creep sensitivity, low warpage and excellent chemical resistance. It shows good mold release, moldability, processability, stiffness and hydrolytic stability. It is suitable for processing by injection molding. It is designed for automotive exteriors & under-the-hood applications such as power distribution, relay and junction boxes. NORYL GTX™ Resin 951W (Asia) is recommended for consumer applications, recreational vehicle, electronics & electrical components and infrastructure.
REQUEST A SAMPLE ORIGINAL DATASHEET CONTACT SUPPLIER
NORYL GTX™ Resin 951W (Asia)
Technical Datasheet | Supplied by SABIC
REQUEST A SAMPLE ORIGINAL DATASHEET CONTACT SUPPLIER
Product Type
  • PPE (Polyphenylene Ether) > PPE Alloy
  • Conductive Resin
Product Status
COMMERCIAL
Geographical Availability
Asia / Pacific
Applications/ Recommended for
  • Automotive
  • Electrical markets > Electrical components
  • Electronics / Computers
  • Households products/ Consumer Goods
  • Automotive >> Under the hood
  • Injection molding - thermoplastics
Key Features
  • Chemical resistance, High
  • Flow, High
  • Heat Resistance, High
  • Heat stabilized
  • Hydrolytically Stable
  • Impact modified
  • Mold Release, Good
  • Moldability, Good
  • Processability, Good
  • Stiffness, Good
  • Unfilled
  • Warpage, Low

NORYL GTX™ Resin 951W (Asia) Properties

Mechanical Properties

Value & Unit
Test Condition
Test Method
Tensile Strain
55 %
(at break, Type I, 50 mm/min) 
ASTM D638
Tensile Strength, Yield
65 MPa
(At 50 mm/min, Type I) 
ASTM D638
Flexural Yield Strength
100 MPa
(At 2.6 mm/min, 100 mm span) 
ASTM D790

NORYL GTX™ Resin 951W (Asia) Processing Guidelines

Injection Molding Properties

Value & Unit
Test Condition
Test Method
Melt Temperature
280 - 310 °C
Nozzle Temperature
270 - 300 °C
Hopper Temperature
60 - 80 °C
Want to list or
update your products?
Want to report errors or
suggest improvements?
Access Reliable
Product Information

Database of 100071 Plastics & Elastomers,
reviewed and updated daily

Improve your Product
Selection Experience

Open your choices, compare products,
ask for samples, contact suppliers

Keep-up with latest
Technical Solutions

Be inspired and never miss again crucial
innovations with our weekly email updates

Back to Top